| Properties and test methods | Unit | Typical Value | Standardization |
| Specific surface area (BET) | m2/g | 170±20 | GB/T20020 |
| pH value (in 4% dispersion) |
3.8 ~ 5.0 | GB/T20020 | |
| Loss on drying (2 hours at 105 °C) |
Wt% | ≤ 0.5 | GB/T20020 |
| Loss on ignition (2 hours at 1000 °C, based on material dried for 2 hours at 105 °C) |
Wt% |
≤ 2.0 |
GB/T20020 |
| Silica content (based on ignited material) |
Wt% | ≥ 99.8 | GB/T20020 |
| Tamped density (based on material dried for 2 hours at 105 °C) |
g/L | 40 ~ 60 | GB/T20020 |
| Carbon content (based on material dried for 2 hours at 105 °C) |
Wt% | 0.7 ~ 1.3 | GB/T20020 |